The column that cannot be unloaded slowly enough
Assumes The columns are shorter than the core and The deflection that arrives three years late.
The bars that take the column over followed a reinforced concrete column through its first fifty years under a steady load. Steel does not creep and concrete does, so as the concrete shortened under its load the bars, bonded to it, shortened with it and took a growing share. At 2 per cent of steel the bars carried a seventh of the load on the first day and more than a third after fifty years. Then that essay took the load away, at once, on the section’s elastic stiffness, and found the bars still squeezed and the concrete pulled into tension by them: −3.0 MPa at 2 per cent of steel, the order of the concrete’s tensile strength.
Columns are unloaded on purpose. A tower is jacked onto a new transfer structure; a damaged column is propped, unloaded and replaced; a building’s load is moved onto temporary works while its foundations are underpinned. In each case the moment of unloading is chosen, and so is its speed. The essay ended on the possibility that a slow unloading, spread over months, would let the concrete creep under its developing tension and relax it as it arose — so that a programme could keep a heavily reinforced column uncracked by taking its load off slowly enough. It needed a calculation in which the history of loading is the unknown’s own, because the single stage of the age-adjusted modulus treats the unloading as something that happens all at once.
Every increment remembered
The calculation here is the step-by-step superposition integral. A concrete’s strain at any time is the sum of the strains caused by every stress increment it has ever received, each through the creep compliance for the age at which it was applied. Eurocode 2 gives that compliance in a form with ageing built in: the instantaneous modulus grows slowly with age, and the creep coefficient for an increment applied at age is reduced by a factor , so concrete loaded late creeps less. Shrinkage is added as a strain of its own, 300 microstrain in the long run, half of it in the first two years. The bars share the concrete’s strain, and at each time the load on the column has to be carried by the concrete’s stress and the bars’ together; that fixes the one new increment of concrete stress at each step.
The arch that waits with its hinges open used the same integral for an arch closed long after it was struck, and the method is the one creep analysis exists for: a history of stress, not a stress. Here it carries one extra burden. The load is taken off over a stated time, from at once to four years, and every decrement is an increment of its own, applied at the age when it happens and creeping thereafter by that age’s compliance. Recovery is the creep of those negative increments. Superposition is known to overstate recovery, since concrete recovers less of its creep than it underwent, and that is the side on which this calculation errs: if anything, it is kind to the slow unloadings.
Two checks hold it in place. With no steel the strain after a year is the compliance times the stress plus the shrinkage, exactly. And with the load held for fifty years the concrete’s stress comes out at 7.72 MPa against the age-adjusted modulus’s 7.73, from a calculation that uses no ageing coefficient at all.
The column unloaded at ten years
The column carries 12 MPa on its gross concrete area from 28 days. Over ten years the concrete’s own stress falls to 7.88 MPa as creep and shrinkage hand load to the bars, which by then carry a third of the column. Unloaded at once, the concrete drops by the elastic share of the load the section takes back, and lands at −2.93 MPa: in tension, held there by bars that are still shortened by ten years of creep. That is essentially the earlier essay’s −3.0.
Unloaded over a month it reaches −2.62, and over a year −2.36. The slower the unloading, the more of the tension the concrete can relax as it develops — the creep of each new tensile increment works against the increment that caused it, as the strain that was imposed showed for a restrained shrinkage, where creep turned a predicted stress of three times the tensile strength into one the concrete survives. A year’s unloading takes a fifth off the peak tension.
Then the three curves meet. Over the following decades the concrete recovers part of its creep, which lets it lengthen against the bars and would relieve the tension, but it also keeps shrinking, which pulls the other way. At 55 years of age all three stand within a few hundredths of −2.20 MPa. The rate of unloading has decided how sharp the peak is and nothing about where the column ends up.
No rate is slow enough
The question was whether a programme could be made slow enough to keep any column below cracking. The answer depends on the steel, and for heavily reinforced columns it is no. At 1 per cent of steel the peak tension is 1.72 MPa at once and the question never arises. At 2 per cent the peak is just under 3 MPa at once and the slow programmes only widen the margin. At 3 per cent the concrete reaches 3.80 MPa at once and 3.04 over a year, so a programme of a little over a year keeps it at its strength. At 4 per cent it is 4.45 at once, 3.53 over a year and 3.39 over four years, and the curve is flattening toward a limit it will not cross: the long-term tension of that column, 3.31 MPa at 55 years of age, which is reached whatever the programme.
So slowness has a floor, and the floor is set before the unloading begins. The concrete’s tension after the load has gone is the concrete’s and the bars’ disagreement about length — the creep and shrinkage the concrete has done that the bars have not — less whatever recovery and relaxation can take back. Unloading slowly buys the relaxation early. It cannot buy more than the column would eventually have anyway, and the slowest programme simply arrives at the long-term state without passing through a peak on the way.
Where the steel decides it
Plotted against the steel ratio, the three thresholds separate cleanly. Unloaded at once, a column of more than 2.1 per cent of steel cracks. Unloaded over a year, one of more than 2.9 per cent. And above 3.3 per cent the column cracks eventually whatever is done, because its long-term tension passes 3 MPa. A programme of unloading is worth the band between 2.1 and 3.3 per cent; below it, unloading at once is safe; above it, nothing in the programme can help, and the cracks have to be accepted, prevented by reloading, or controlled by the bars themselves.
That last option is the ordinary one. Columns of 3 and 4 per cent of steel are common in the lower storeys of towers, and their tension cracks would be fine, distributed by the bars, of no structural consequence to a column that is to carry compression again. The steel the concrete asks for set out how much reinforcement keeps a crack fine; a heavily reinforced column has much more than that. What the cracking matters to is durability, for a column exposed to weather or chlorides, and a column that will never be reloaded — one being taken out of service — where the cracks are the column’s state from then on.
A young column is better unloaded at once
The longer the load has been held, the more creep the concrete has done and the more the bars have taken, so the tension left by unloading grows with the age at which it comes off: −1.34 MPa at once after three months, −2.93 after ten years, −3.06 after thirty. Most of it is in place within a few years, since creep under a sustained load slows with time.
The surprise is at the young end. Unloaded at three months, a year-long programme leaves −1.63 MPa, more than unloading at once. A young concrete is still drying fast, and its shrinkage during the year of unloading adds tension faster than its creep relieves it; the bars resist the shrinkage as they resisted the creep. An old column has done most of its shrinking, so the year of unloading is a year of relaxation only. The rule that slow is gentle is a rule about old concrete, and a column unloaded within its first year or two — a temporary propping in construction, an early transfer — is better unloaded at once and left to relax.
The programmes a site can actually run
The rates in these figures run from an instant to four years, and only part of that range is available on a site. A column unloaded by jacks onto a transfer beam or a set of props comes off in hours: the jacks are pumped, the load moves, and the column is left. A building whose load is moved onto temporary works floor by floor, as a frame is demolished from the top, loses its load over weeks. Only a deliberate programme — a column relieved in stages over months while its replacement is built alongside — gets into the range where slowness is worth having, and it pays for every month in the cost of the temporary works that carry the load meanwhile.
On the 2 per cent column the arithmetic of those programmes is plain. Hours are the instant case, −2.93 MPa, just inside the concrete’s strength. A month gives −2.62, which is a useful margin for a column whose strength is uncertain or whose surface has been weakened by drying. A year gives −2.36, and buys only another 0.26 MPa for eleven more months of propping. The return falls away quickly, because the tension’s own creep, like every creep, does most of its work early: more than half of what a year buys, a month has already bought.
On a 4 per cent column — the lower storeys of a tower, where columns are packed with steel to keep them slender — no programme helps. The column will reach −3.31 MPa within decades whatever is done, and the only questions are whether its cracks will be fine and whether they matter. The decision is about the column’s future, not its unloading. A column that will be reloaded can be unloaded at once, since its cracks will close again under compression; one that will not can be unloaded at any rate and should be expected to crack.
There is a third choice, and the propping that the backprop that takes load nobody gave it examined is the familiar form of it: never to take the load entirely off. A column left with part of its load keeps its concrete in compression only if the residual load is enough to cancel the disagreement the bars hold, and on a heavily reinforced column that is a large part. Left at 45 per cent of its load, the 4 per cent column’s concrete stands at +0.13 MPa just after the partial unloading and +0.49 decades later; at 40 per cent it starts at −0.35 and creeps back to zero; at 30 per cent it is in tension from the start and stays there. Nearly half the load has to stay on a column with that much steel to keep its concrete out of tension, which is a measure of how much of the column the bars have taken over in ten years.
The tension that drying keeps up
Separating the two causes shows what the floor is made of. Without shrinkage the same column unloaded at once reaches −2.11 MPa and relaxes to −1.27 over the following decades, as creep recovery and the tensile creep of the concrete do what they would be expected to. With shrinkage it reaches −2.93 and relaxes only to −2.20. Of the long-term tension, about 0.9 MPa is the bars resisting the concrete’s drying, and that part is independent of any load: a column that was never loaded at all, with 2 per cent of steel, carries a tension from its own shrinkage.
This is the thermal-compatibility problem of the coincidence reinforced concrete stands on, with the drying of the concrete in place of a temperature: two materials bonded together that want different lengths. The load’s creep adds to the disagreement and the unloading reveals it. A slow unloading can relax the part of the disagreement that creep made, but not the part that drying keeps making.
What the floors above are left with
The column’s shortening is the other half of the story, and it is what the structure above notices. Over ten years the column has shortened by 1,030 microstrain, 3.7 mm in a 3.6 m storey, and the floors it carries have followed it down; the floor that is level on one date found how that is compensated in construction. Unloaded at once, the column springs back elastically to 733 microstrain and then recovers slowly, to 550 by 55 years of age, while shrinkage holds part of the shortening permanently. The floors above rise by 1.7 mm per storey over the decades, not all at once.
Put half the load back a year after unloading, as happens when a column is propped for a repair and then returned to partial service, and the column shortens again under the new load, creeping as a much older concrete creeps: at 55 years it is at 808 microstrain, 2.9 mm a storey. The reloaded column does not return to its original shortening, because the new load creeps less than the first did, but neither does it keep the recovery it had begun. A tower whose column is unloaded and partly reloaded has a floor that moves up and then down by millimetres a storey over years, against neighbours that did neither.
The calculation’s assumptions, named
The creep model is Eurocode 2’s, with its ageing function and a single notional size, and the column is uniform: no difference between the core of the section and its surface, which dry and creep at different rates. A real column’s surface shrinks first and cracks first, often before any unloading, under the restraint of its own core, and that is outside a model that gives the section one strain. The tensile strength is a single value, 3 MPa, with no account of its own increase with age or its reduction under sustained tension, and the column that fails years later is a reminder that concrete’s long-term strength under sustained stress is not its short-term one.
Superposition overstates recovery, which flatters the slow unloadings and the long-term relaxation; a model with less recovery would leave every curve a little lower after unloading and the floor a little nearer the instant value. The bars are elastic throughout, which they are here, at stresses well below yield. And the load is axial and uniform: a column unloaded by jacking at its head, with its bars continuous through the jacking point, is the case computed. A column cut and propped carries its load differently, through the props, and its bars may not be continuous at all.
A disagreement about length
The tension in an unloaded column is a disagreement between the concrete and its bars about how long the column should be, and it is made by creep and shrinkage over the years the load was held. Unloading does not create it; unloading reveals it, by taking away the load that was holding the concrete in compression against it. A slow unloading lets the concrete relax some of the disagreement as it is revealed, and that is worth up to a fifth of the peak tension for a column that has done its shrinking. It is not worth more, because the column’s long-term state is fixed by what has already happened, and the slowest possible programme arrives there with no peak at all. Above about 3.3 per cent of steel that state is cracked. Below about 2 per cent it never was in danger. The programme is a choice only in between.
Still open: the column whose surface has already cracked
Every number here belongs to a section with one strain, uncracked until its whole area reaches the tensile strength. A real column’s skin dries years ahead of its core and is restrained by it, and by the time the column is unloaded the surface may be crazed with fine shrinkage cracks while the core is still in compression. Unloading then adds a tension that finds those cracks first. Whether a column whose surface has already cracked from drying crosses its tensile strength earlier when unloaded, because its skin no longer carries tension, or later, because its core has dried less and carries less of the bars’ disagreement, needs the section divided into layers that dry and creep at their own rates.
Named alongside this one
Essays reaching for the same objects. Nobody chose these; they are what the concept index makes visible.
- The arm connected late creep · differential shortening · shrinkage
- The curvature nobody applied creep · differential shortening · shrinkage
- The same steel, and a wider crack reinforcement ratio · shrinkage · tensile strength
- Stiffer than its cracked section says creep · tensile strength
- The angle made in the casting yard creep · shrinkage
- The arm that calls for its own visit creep · differential shortening
The objects this essay names
Each one links to every other essay that touches it.
Age-adjusted effective modulusAgeing coefficientCreepDifferential shorteningReinforcement ratioShrinkageTensile strength