The joint born holding a moment
Assumes The angle nobody limits, The deflection that arrives three years late and The moment over the support, and what it buys.
The joint cast over the pier found that two precast pretensioned beams made continuous over a pier by casting a joint between them do not stay at the moment the joint was cast with. The beams go on cambering upward as their prestress creeps, the slab cast on top shrinks against them and bends them down, and the joint, which now holds their two ends at one rotation, turns whatever change of free rotation is still to come into a restraint moment. A joint cast at six weeks, while the beams are young and their creep camber still growing, ends thirty years later sagged by 160 kN·m; one cast at a year, when the camber has slowed and the slab’s shrinkage has the upper hand, ends hogged by 214; the balance is at about 113 days. The joint poured twice over the pier tried casting the joint in two stages, hoping the early pour would hold the creep and the late one escape the shrinkage, and found that the composite section holds what a single pour on the slab’s day would have held regardless.
Both essays treated the moment as something the programme decides. The second ended on the alternative that the arm connected late found in an outrigger, where a connection’s force can be set by jacking at the moment it is made: lift or lower the beams’ pier ends on jacks before the joint is cast, let them down once it has hardened, and the joint is born holding a chosen moment, with the restraint laid over it. If the chosen moment is the opposite of what the restraint will bring, the two should cancel at thirty years, and the slab’s date would no longer matter. Whether they do, or whether the jacked moment relaxes away like everything else the joint holds early, is the question.
A moment that nobody’s load put there
The beams are the earlier essays’: two 12 m pretensioned beams, 300 mm wide and 700 mm deep, with a 160 mm slab 1.2 m wide, in 60 per cent humidity, made continuous in a single pour of joint and slab. The restraint moment is found by the same step-by-step creep integral: every increment of free end rotation after the pour becomes an increment of moment on the composite section, per radian for two equal spans, and each increment then relaxes by the beams’ creep from its own age.
A jacked moment enters the same calculation in one line. Holding the beams’ pier ends up by while the joint hardens and then letting them down puts the pier support of a two-span continuous beam below where it was when the beams became continuous, which is a sagging moment at the joint of ; holding them down, or lifting the far ends, puts hog. Either way it is an imposed deformation, applied on the joint’s first day and held from then on, and the composite section answers it with a moment that relaxes by the creep integral of a unit step at that age, . The joint’s moment is then
and a jack that cancels at thirty years has . On this section, 20 mm of jack movement is about 400 kN·m.
Jacked and unjacked, over thirty years
The jacked histories end at nothing, as they were built to, and they start a long way from it. The six-week joint begins its life hogged by 413 kN·m, and over thirty years the restraint’s sag and the jack’s relaxation bring it up to zero together. The year-old joint begins sagged by 407 and falls to zero. The unjacked histories, dashed, are the earlier essays’ — the young joint creeping into sag, the old one shrinking into hog — and the jack has not removed them; it has started each joint from the opposite side of nothing, far enough out that the restraint arrives back at the middle.
Both jacks are about twice the moment they cancel. That ratio is the jacked moment’s own relaxation.
How much of a jack the joint keeps
A jacked moment is held by concrete that creeps, and concrete that creeps under a held deformation relaxes the stress that holds it — the same creep that brings the deflection that arrives three years late under a held load. The relaxation curve is the creep integral of a unit step: it starts at one on the day the jacks are let down, falls fast in the first months while the beams are young, and is still falling slowly at thirty years. A joint cast at six weeks keeps 0.39 of its jacked moment; one cast at a year, when the beams’ creep coefficient for a new load has fallen, keeps 0.53. A jack must therefore be 1.9 to 2.6 times the moment it is meant to cancel, and that factor is the same physics as the restraint itself: the restraint moment is small precisely because it is built from increments that relax, and the jack, applied all at once at the start, relaxes most.
That is the difference between jacking a connection and jacking a continuity joint. A jack that sets a force in a member which does not creep keeps what it put in; a jack that sets a moment in a concrete joint is a load on the very material whose creep it is trying to anticipate, and the creep it anticipates is also the creep that takes it away.
The jack that cancels, slab day by slab day
The jack needed is a mirror of the unjacked moment, magnified by one over the relaxation. For an early slab it is a hog, for a late one a sag, and at the balance age of 113 days it is nothing, because there is nothing to cancel. So the jack does answer the earlier essay’s question in one sense: for any slab date there is a jack that cancels at thirty years, and it is read off this figure on the day the slab is poured, when the date is no longer a forecast.
The two horizontal lines are what the joint can carry before it cracks. In sag the joint’s tension is in the beams’ bottom connection — the bars or strands that tie the two beams’ bottom flanges across the diaphragm — and it cracks at 140 kN·m. In hog the tension is in the slab’s top, which cracks at 239. The jacks that cancel are outside both lines for every slab date except a band of a few weeks either side of the balance age. A joint cast at four weeks would be born hogged by 591 kN·m, two and a half times the slab’s cracking moment; one cast at a year sagged by 407, nearly three times the bottom connection’s. The jack that cancels is not an adjustment. It is a load larger than any the joint will see in service.
What a jack that may not crack the joint can do
A designer who will not crack the joint on its first day can still jack it as far as its cracking moment, and the figure draws what that buys. Jacked to the slab’s 239 kN·m of hog, the six-week joint ends at 67 kN·m of sag instead of 160: the jack takes away 58 per cent. The four-week joint, whose cancelling jack would be 591, ends at 126 instead of 211. On the late side the joint’s limit is the bottom connection’s 140 kN·m of sag, the weaker of the two, and the year-old joint ends at −140 instead of −214, a third removed. Near the balance age the jack needed is small enough to apply in full and the joint ends at nothing.
Held to what the joint can take uncracked, a jack cancels about half the restraint for an early slab and a third for a late one. That is a useful reduction and a different design statement from the one the jack promised. It turns a joint that would have been sagged by 160 into one sagged by 67, which may be the difference between a bottom connection that cracks in service and one that does not; it does not make the slab’s date irrelevant.
The jack and the humidity it was set for
The jack is set from a prediction of creep, and creep depends on the humidity the beams actually live in, which a designer can only guess. The figure sets each jack for 60 per cent and lets the beams creep at 45 to 80. For the early slab the jack is robust: the jacked joint ends between −1 and 30 kN·m across the whole range, where the unjacked one ranged from 158 to 208. The restraint and the jack’s relaxation move together with humidity — damper air means less creep, so less restraint and also less relaxation of the jack — and their errors largely cancel.
For the late slab they do not. In damp air the year-old joint’s restraint falls to −106 kN·m, half what it is at 60 per cent, because its hog comes mostly from the slab’s shrinkage and a damp slab shrinks less; but the jacked sag relaxes less in damp air too, and the two errors add. At 80 per cent the jacked joint ends sagged by 126 kN·m, more than the unjacked one is hogged. A jack is an imposed deformation sized against a prediction, and its error scales with its own size, which is two to three times the moment it cancels. Where the restraint and the jack relax by the same mechanism, the errors cancel; where the restraint is mostly shrinkage and the jack mostly creep, they do not.
Why a closure jack was robust and this one is not
The humidity figure’s contrast has a precedent worth setting beside it. The jack that creep carries past the mark jacked the closure of a prestressed beam built from both ends, so that it would start with the secondary moments it would have had if it had been stressed all at once, and found the setting good to a couple of dozen kN·m for creep coefficients a third either way. Its jack and the moment it corrected were both creep: the staged deficit creeps back toward the at-once moments as while the jack relaxes as , and an error in moves both the same way. The correction was robust because the thing corrected and the thing correcting obeyed one law.
The continuity joint’s early slab is the same case. Its restraint is mostly the beams’ creep camber after the pour, and the jack relaxes by the beams’ creep, so a damper year that gives less creep also gives less relaxation and the two errors cancel: −1 to 30 kN·m across the whole range of humidities. The late slab is a different case. Its restraint is mostly the slab’s shrinkage bending the composite section down, and shrinkage is a strain the slab imposes on itself, with a dependence on humidity much steeper than creep’s. The jack still relaxes by creep. In damp air the shrinkage falls by half while the share of the jack that survives rises by less than a tenth, 0.53 to 0.57, and the jack — sized for a shrinkage that did not happen — is left holding most of itself. A jack is robust only against the mechanism that relaxes it, and on a late joint that is not the mechanism that made the moment. That is also why the strain that was imposed needed creep and shrinkage together to predict a restrained member’s stress: they are opposite in sign and comparable in size, and neither is known to better than a fifth.
The span changes which side the jack is on
The beams here are one section at one span, and a longer span changes the balance between what cambers the beams up and what bends them down. Self-weight’s moment grows as the square of the span, the prestress’s camber does not, so a longer beam’s creep camber is smaller, and its young joint’s sag smaller with it; at about 18 m the six-week slab’s restraint has almost vanished, and the jack it needs is a fifth of the slab’s cracking moment. Past that the young joint’s restraint changes sign and the jack is a sag again. The late slab goes the other way: a year-old joint’s hog grows with the span, and the jack that would cancel it rises to 4.7 times the bottom connection’s cracking moment at 20 m.
Read with the cracking limits, the figure says when a full jack is possible: for an early slab on a span where the restraint has nearly balanced itself, which is exactly when a jack is least needed. The case the jack was meant for — the late slab on a long span, the joint the programme forced — is the one where it is furthest out of reach.
The jack, by hand
The whole result follows from two numbers. The first is the restraint at thirty years, the earlier essay’s 160 kN·m for the six-week joint. The second is how much of a moment applied on the joint’s first day survives thirty years of the beams’ creep. Eurocode 2’s creep coefficient for a load applied to these beams at six weeks is 1.31, and the usual age-adjusted shortcut for a held deformation, , gives 0.49; the step-by-step integral, which loads each increment of moment at its own age and lets it creep from there, gives 0.39, and it is the integral’s number the figures use. A jack that cancels must be times the restraint — about 410 kN·m on the integral, 330 on the shortcut — so even the generous estimate puts the jack well past the slab’s cracking moment of 239. The conclusion does not depend on which relaxation is right.
The hand version also says what would change the answer. A jack applied later, once the joint’s concrete and the beams are older, relaxes less, but the restraint it must cancel is then smaller too. A jack applied in two steps — part at the pour and the rest a year later, when much of the creep has gone and the remaining relaxation is small — would need less total movement and cross the cracking moments less, because a step applied at a year keeps about half of itself rather than two fifths. That is the jacked outrigger’s re-shimming arriving at a concrete joint, and it is not drawn here.
What the jacked joint leaves out
The jacked moment is taken as a single imposed deformation of the composite section on the day of the pour. In practice the joint hardens over a few days and the jacks are let down a week or two after casting, so the deformation is applied to a section whose joint concrete is young and soft, and the composite section’s stiffness at release is less than its 28-day value; the jack would then relax faster at first and the factor be larger still. The joint is also taken as uncracked throughout, which is the point of holding the jack to the cracking moments: a joint jacked past them would crack and lose stiffness, and its restraint would then follow a different, softer history that the creep integral of an uncracked section cannot represent.
The beams are equal and the pier symmetric. A pier between unequal spans, or a viaduct of several spans each jacked at its own pier, would need the jacks chosen together, since a jack at one pier moves every support moment along the line — the problem the angle nobody limits and its rotations pose at a bearing, and that a continuous truss’s jacking order poses at its piers. And the creep and shrinkage are Eurocode 2’s mean functions, with no scatter but the humidity’s; the real scatter of creep is about 20 per cent either way, which the humidity figure is a stand-in for, and the late slab’s sensitivity to it is the figure’s warning.
Still open: the joint jacked twice
Everything here jacks the joint once, at the pour, against a forecast of thirty years. The jacks could equally be left in place under the beams’ pier ends for the joint’s first year, reading the support reaction — which is the joint’s moment in another form — while the creep happens, and be adjusted once more when the readings show where the joint is going. A second adjustment at a year keeps about half of itself rather than two fifths, so it can be smaller than the first and still cancel, and it is set against a creep that has already been partly measured rather than predicted. Whether two jacks, the first held to the joint’s cracking moment and the second correcting what the first year revealed, can bring a late slab’s joint to nothing at thirty years without cracking it, and whether a reading of the reaction at a year predicts the remaining twenty-nine well enough to set the second, is what leaving the jacks in would ask of the angle made in the casting yard and the creep that made it.
Named alongside this one
Essays reaching for the same objects. Nobody chose these; they are what the concept index makes visible.
- The prestress the member takes back creep · prestress · relaxation · shrinkage
- Four inequalities and a wedge creep · prestress · relaxation
- The arch that waits with its hinges open creep · relaxation · shrinkage
- The beam built towards its own middle continuity · creep · prestress
- The beam stressed one bay at a time continuity · creep · prestress
- The hanger that loses force and keeps its stiffness creep · prestress · relaxation