The slab left to dry before the fill
Assumes The load that depends on what carries it, The deflection that arrives three years late and The pressure the roller leaves behind.
A basement wall propped at its top by its ground slab has been followed through three essays, each changing its mind about what holds that top. The prop that holds what the roller left found that a stem propped by its ground slab before its fill goes up keeps the pressure the compaction roller locks into the fill: a propped stem cannot move away from the fill to relax it, so the residual stays as a force in the prop and a moment in the stem much smaller than an unpropped one’s. The slab that shrinks away from the wall then found that the prop is a concrete slab, and a concrete slab shrinks. Its end draws back from the stem by millimetres over years, and once it has drawn back about two millimetres the stem has nothing to lean on: it has relaxed its residual, bent to the unpropped shape, and is carrying the unpropped moment. And the seasons that stop reaching the wall added the slab’s yearly swing with temperature on top of its shrinkage, which pushes the slab back toward the stem each summer, and found that the seasons stop reaching the stem within a couple of years of the fill.
Every stem in those essays was filled while its slab was young. The slab was cast four weeks before the fill was finished, and so almost all of its drying shrinkage was still to come when the residual was locked against it. That essay ended on the obvious remedy: cast the slab, wait while it dries, and only then put up the fill, so that the roller’s residual is locked against a slab that has done most of its shrinking. Whether that keeps the residual in the prop for the building’s life, whether the stem then carries the propped moment it was designed for, and whether the price of the delay is a prop force that never relaxes, is the question here.
The same stem, filled late
The stem is the one the three earlier essays shared: 3 m high, fixed at its base, its fill of unit weight 20 kN/m³ placed in 250 mm lifts and rolled at 60 kN/m. Its top is held by a 250 mm ground slab spanning 30 m between this wall and the one opposite, in an interior at 60 per cent humidity. The slab’s end moves away from the stem by half the slab’s shrinkage strain times its length, and back and forth by its seasonal swing — 3 K either way each year, at /K — and at each moment the stem is solved against wherever the slab end then is: bearing while the slab reaches it, slack once it has drawn away.
The one new thing is the date of the fill. The slab’s shrinkage is Eurocode 2’s, drying from one face from day seven, with a notional size of 500 mm for a 250 mm slab that dries from its top only. What moves the slab away from the stem is the shrinkage after the residual is locked in, , so delaying the fill is simply starting the clock later on the same curve.
A later fill leaves less to shrink
The stem lets go of the slab at 2.08 mm. That number is the stem’s, not the slab’s: it is how far the stem’s top can follow the slab outward, relaxing the residual and bending under the fill, before the stem reaches the shape it would have had with no prop at all. It is the same for every delay, and the figure’s dashed line is where each curve has to stay below for the slab to keep any grip.
A fill at four weeks leaves the slab 4.42 mm of shrinkage still to do over thirty years, twice the stem’s slack, and it crosses the line in sixteen months. A fill at six months leaves 3.14 mm and crosses after 5.3 years. A fill at a year leaves 2.36 mm, which is more than the slack, and yet the slab still touches the stem in the thirtieth year: the seasonal swing brings the end 0.45 mm back toward the stem each summer, and a slab whose shrinkage since the fill is less than the slack plus that half-millimetre touches the stem once a year for ever. A fill at two years leaves 1.57 mm and stays inside the slack at its furthest.
Six months of drying buys four years of contact; a year buys thirty. The steepness of that step is the shrinkage curve’s shape and is worth understanding before trusting it, which the hand budget below does.
What the prop actually holds
Contact and force are different things, and the earlier essays’ conclusion that the residual cannot come back is what separates them. The roller’s residual, 22.6 kN/m at the prop, is a force the fill holds because the stem has not moved. As the slab draws back the stem follows, and every millimetre it follows relaxes the fill’s locked-in pressure in proportion. When the summer pushes the slab back, it can push the stem back only to where the residual was relaxed from; it cannot re-lock pressure the fill has let go of, because nothing compacts the fill again. So the force in the prop is set by the slab’s furthest point so far, not by where it is today.
That is why the year-late fill, which touches every summer, holds 3.4 kN/m after five years and nothing after twenty. Its slab has drawn back past the point where the residual is gone, and what it touches each summer is a stem that has nothing left to give it. The two-year fill does better: 11.1 kN/m after five years, half the residual, and 6.3 after twenty. The prop’s force relaxes whatever the delay — the delay sets how far, not whether — so the price of a late fill is not a prop force that never relaxes. It is a prop force that relaxes more slowly, and for the stem that is a different and less useful thing.
The moment the stem carries in its tenth year
The stem’s design question is the moment at its base, because that is where the bars are. Propped, the stem carries 26.6 kN·m/m: the propped cantilever’s moment under the fill’s pressure with the residual held. Slack, it carries 69.6: the free cantilever under the same fill, the residual relaxed. A stem detailed for the propped moment has a third of the steel a slack one needs, which is the reason anybody would prop it.
Every year has a worst moment, and it comes when the slab is furthest from the stem — in winter, when the slab is cold and contracted. For the three earlier fills that is the slack moment from the first few years on: once the slab has drawn back past 2.08 mm in any winter, that winter the stem is a cantilever. Even the two-year fill, the only one whose slab never draws past the slack, reaches 63.0 kN·m in the tenth year, nine tenths of the slack value, because the stem’s base moment rises steeply as its top is let go: a slab that draws back most of the way to the slack has taken most of the way to the slack moment with it. By the thirtieth year it is 68.4.
A stem whose slab still bears on it every year is not a propped stem. The contact the delay buys is contact at the slab’s nearest; the design needs it at the slab’s furthest. A stem that is to be designed for 26.6 kN·m needs a slab that in its coldest winter has drawn back by only a small part of the 2.08 mm, and a ground slab cannot promise that on any schedule a contractor would accept.
The shrinkage the fill has to wait for
The step from five years to thirty between a six-month fill and a one-year fill can be had by hand, and doing it shows where the steepness comes from. The slab end touches the stem in a summer as long as the shrinkage since the fill, times the slab’s half length, is less than the stem’s slack plus the swing:
On this slab is 15 m, the slack 2.08 mm and the swing 0.45 mm, so the shrinkage allowed after the fill is microstrain. The slab’s thirty-year shrinkage is about 341 microstrain; it must already have done 172 of them when the fill goes up. Eurocode 2’s drying function has the shape , and with a notional size of 500 mm the time constant is 447 days: a thick slab drying from one face is half-dry at about fifteen months, not in weeks. That is the whole of the result. A slab that will do half its shrinkage in a year and a quarter cannot be made to have done it in six months, and the fill has to wait for the curve, not for the calendar.
The hand budget says ten months; the stem’s own history says between six months (still losing the slab at 5.3 years) and a year (touching for thirty). They agree because they are the same inequality, and the only thing the history adds is the stem’s nonlinear relaxation between the two. What the budget makes plain is that every quantity in it is a length times a strain: double the slab’s length and the allowed strain halves.
Months of delay against years of contact
The contact time is a threshold, not a slope. For each slab there is a delay below which the slab lets go within a few years and above which it touches for the building’s life, and the transition is a few months wide because the shrinkage still to come falls through the budget while the curve is still steep. The 20 m slab needs very little — its allowed strain is half as large again as the 30 m slab’s — and the 40 m slab needs more than a year: filled at a year it lets go after 8.3 years, filled at three it holds.
How long each slab must dry
Read the other way round, the figure is a design rule for when the delay is worth having at all. A slab up to about 15 m between walls never draws far enough to lose the stem, whatever the date: even after a four-week fill, the 295 microstrain it has still to shrink, times 7.5 m, is 2.2 mm, inside the slack plus that slab’s swing. Past that the delay rises quickly with length and falls quickly with humidity, because humidity sets the size of the shrinkage, and a slab in a damp basement at 80 per cent shrinks so little that two months of drying is enough for 30 m. A dry, heated interior at 50 per cent is the worst case and needs the longest wait.
Read as a schedule it is less forgiving. Ten months between casting a ground slab and backfilling against the walls it props is the whole superstructure’s duration on many buildings, and the slab was cast early precisely so that the fill could go up and the site be cleared. And even that wait buys only the contact of the earlier figures — touching every summer, holding a little force for a decade, and carrying nearly the unpropped moment every winter.
A joint is worth ten months
The figure of delays against lengths contains a cheaper answer than waiting, and it is worth drawing out because it costs nothing in programme. What the stem feels is the shrinkage of the slab between itself and the nearest point that does not move toward it, and for a slab running wall to wall that point is the slab’s middle, 15 m away. A pour strip or a movement joint parallel to the wall, a few metres in, makes that distance the strip’s: the slab beyond the joint shrinks toward its own middle and pulls its edge away from the joint, not from the wall. The 30 m slab then behaves, at the stem, like the 15 m slab of the figure, and a 15 m slab needs no delay at all.
Put as arithmetic, the budget inequality is linear in . Halving the distance to the slab’s still point halves the movement, doubles the shrinkage the slab may still do after the fill, and turns 168 microstrain into 336 — very nearly the whole of the slab’s thirty-year shrinkage. A slab cast four weeks before the fill, with a joint 7.5 m from the wall, keeps the stem in contact every summer for thirty years, which the undivided slab needed ten months of drying to do. The bay cast late in the bay that is cast last is the same device used against a different restraint: a gap that takes the shrinkage of the part that has already shrunk out of the part that matters.
It is not a full answer, for the same reason the delay was not. A joint shortens the slab’s movement at the stem but does not remove it, and the prop’s force still relaxes through the winters; a stem behind a 15 m slab still carries most of the slack moment by its tenth year in the coldest weather, for the reasons the moment figure gave. What the joint buys is the delay’s benefit without the delay — contact without a ten-month wait — and the stem’s design still has to be made for a top that moves.
What the remedy really is
What the delay cannot change is the ratio that decides everything: a ground slab moves by millimetres, and a 3 m stem propped at its top can follow the slab by only a couple of millimetres before it has given up the whole of what the prop was for. Every remedy that works changes one side of that ratio. A movement joint in the slab near the wall, cast late, cuts to the joint’s distance. A slab tied to the stem by bars across the joint turns the stem’s top into part of the slab, which then shrinks with the stem’s top rather than away from it, and the shrinkage restraint becomes the slab’s problem — cracking in the slab instead of moment in the stem, which is the trade the strain that was imposed prices. Or the stem is designed for the slack moment, which is what a stem whose slab is a prop only by courtesy is.
There is a fourth, and it is the cheapest: do not count on the compaction residual being held at all, and design the stem as propped against the fill’s at-rest pressure alone, which the slab’s shrinkage does not take away because at-rest pressure does not depend on the stem staying put. That is what the pressure the roller leaves behind and the stem that bends away from the roller together imply: the residual is real, large and fragile, and the prop that is supposed to keep it is the most movable thing in the basement.
The fill, the slab and the stem: three histories in one inequality
The whole argument fits in the budget inequality, and each term in it has its own history the figures simplify. The slack, 2.08 mm, is the stem’s: it would be larger for a more flexible stem, which relaxes its residual over a longer movement, and smaller for a stiffer one. The swing is the building’s: a heated interior swings less than 3 K a year, a ventilated car park more. And the shrinkage is the slab’s, for which Eurocode 2’s curve is a mean with a scatter of about 30 per cent either way; a slab that shrinks 30 per cent more than the mean needs the fill delayed by about as much again as the curve suggests, because the delay must be found on a curve that flattens.
The model also takes the slab’s end to move freely, its whole half-length’s shrinkage arriving at the stem. A ground slab on a subgrade is held by friction along its length, and friction restrains the shrinkage near the slab’s middle more than near its ends, so the end moves less than the free strain says, and a slab with a membrane under it moves almost freely. Neither the friction nor the slab’s own cracking — which, once a ground slab cracks across, divides it into lengths that each move by their own half-length — is drawn here. Both reduce the movement; neither changes the conclusion that the movement is measured against a slack of two millimetres.
Still open: the prop that is a slab tied to the stem
The remedies above all treat the slab as something that pushes on the stem and can draw away. A slab tied to the stem by starter bars cannot draw away: its shrinkage then pulls on the stem’s top instead of releasing it, and the stem is dragged toward the slab’s middle, away from the fill. That relaxes the residual even faster than a slab that lets go — a stem pulled 2 mm away from its fill by its own slab is as slack as one left behind by it — but it does so while the bars across the joint carry the slab’s restrained shrinkage, and they crack the slab near the wall in its first years. Whether a tied slab is then a prop that relaxes the residual on day one and holds the stem’s top against the fill’s later creep, or whether the cracked joint lets go in the same two millimetres, is the question that tying the slab to the wall puts to the prop that holds what the roller left.
Named alongside this one
Essays reaching for the same objects. Nobody chose these; they are what the concept index makes visible.
- The gap nobody computed shrinkage · thermal movement
The objects this essay names
Each one links to every other essay that touches it.