Series

Creep buckling — the series

One essay so far on this idea, and more questions about it than one essay answers.
  1. The deflection goes on growing, and sometimes it does not stop. Second-order deflection of a sustained-loaded concrete column against age, on a log time axis. Creep takes the effective modulus down, which takes the buckling load down with it — from 11580 kN on the day to 3309 in the long term, 29 per cent of it — so the amplifier 1/(1 − N/N_cr) grows even though nothing was added to the load. At 2200 kN the column settles: 25 mm of eccentricity on the day and 60 mm at the end, a factor of 2.4 for a load that never changed. At 5294 kN — still only 46 per cent of the day-one critical load — it does not settle, and the divergence arrives at 55 days for no new reason at all.

    The column that fails years later

    A concrete column under sustained load goes on straining at constant stress, so its deflection grows — and because the second-order moment is the load times that deflection, the demand grows with it. There is a load below which the two settle and one above which they never do.

    part 1 · stability

All series